Plastic plating-plating acid bright copper\ nickel\ gold\ tin electroplating process

Plastic plating-plating acid bright copper\ nickel\ gold\ tin electroplating process.
Huizhou Boluo Tenglong Technology Co., Ltd. serves you wholeheartedly! Mainly engaged in plastic hydroelectroplating processing, with plastic injection molding processing, mold processing and so on!
one.. Classification of electroplating processes:
Acid Bright Copper plating Nickel / Gold Tin plating.
two.. Technological process:
Pickling "full plate copper plating" pattern transfer "acid deoiling" two-stage countercurrent rinsing "micro-etching" two-stage pickling "tin plating" secondary countercurrent rinsing.
Countercurrent rinsing "pickling" pattern electroplating copper "two-stage countercurrent rinsing" nickel plating "two-stage water washing" leaching citric acid "gold plating" recovery "grade 2-3 pure water washing" drying.
three.. Process description:
(1) pickling.
1 function and purpose:
Remove the oxides on the plate surface, activate the plate surface, the general concentration is 5%, and some keep it at about 10%, mainly to prevent the water from being brought into the tank and cause the instability of sulfuric acid content in the bath.
2 acid leaching time should not be too long to prevent plate oxidation; after using for a period of time, when the acid solution is turbid or the copper content is too high, it should be replaced in time to prevent pollution of electroplated copper cylinder and plate surface.

3 C.P grade sulfuric acid should be used here.
(2) full-board copper plating: also called copper, plate electricity, Panel-plating.
1 function and purpose:
Protect the thin chemical copper just deposited, prevent it from being eroded by acid after oxidation, and add it to a certain extent by electroplating.
2 process parameters related to copper plating on the full plate: the bath solution is mainly composed of copper sulfate and sulfuric acid, and the formula of high acid and low copper is adopted to ensure the uniformity of plate thickness distribution and the ability of deep plating on deep holes during electroplating; the content of sulfuric acid is mostly 180 g / liter, and most of them reach 240 g / L; the content of copper sulfate is generally about 75 g / liter, and a small amount of chloride ion is added to the bath solution to play a glossy effect as an auxiliary gloss agent and copper gloss agent. . The temperature of the copper cylinder is maintained at room temperature, the general temperature is not more than 32 degrees, and most of the temperature is controlled at 22 degrees, so it is recommended to install a cooling temperature control system because the temperature is too high in summer.
3 process maintenance:
Replenish the copper gloss agent according to kiloampere hours every day, add it according to 100-150ml/KAH; check whether the filter pump is working properly and have air leakage; scrub the cathode conductive rod with a clean wet dishcloth every 2-3 hours. The contents of copper sulfate (once a week), sulfuric acid (once a week) and chloride ion (twice a week) in the copper cylinder should be analyzed regularly every week, and the light agent content should be adjusted through the Hall cell test, and the relevant raw materials should be replenished in time. Every week, the anode conductive pole and the electric joint at both ends of the tank body should be cleaned, and the anode copper ball in the titanium basket should be replenished in time, with low current 0. 2murine 0. 5ASD electrolysis 6Mel 8 hours; every month should check whether the anode titanium basket bag is damaged, the damaged should be replaced in time; and check whether there is anode mud accumulated at the bottom of the anode titanium basket, if so, clean it up in time; and use carbon core to filter 6Mel continuously for 8 hours, while low current electrolysis to remove impurities; decide whether large treatment (activated carbon powder) is needed according to the tank liquid pollution every half a year or so; replace the filter element of the filter pump every two weeks;].
4 major processing programs: A. Take out the anode, pour it out, clean the anode film on the anode surface, then put it in the barrel of the packing copper anode, coarsening the copper corner surface to a uniform pink with a micro-etching agent, rinse and dry, put it into the titanium basket and put it into the acid tank to spare B. Soak the anodic titanium basket and anode bag in 10% lye for 8 hours, rinse dry, then soak with 5% dilute sulfuric acid, rinse and dry. Transfer the bath liquid to the spare tank, add 30% hydrogen peroxide of 1-3ml/L, and begin to heat up. When the temperature rises to about 65 degrees, turn on the air and stir for 2-4 hours; D. Turn off the air stirring and slowly dissolve the active toner into the bath solution by 3m / L 5g / L. after the solution is completely dissolved, turn on the air stirring and keep it warm for 4 hours. Turn off the air stirring, heating, let the active toner slowly precipitate to the bottom of the tank; F. When the temperature drops to about 40 degrees, use 10um's PP filter element to add filter powder filter solution to the clean work tank, open the air stirring, put it into the anode, hang it into the electrolytic plate, press 0. 2-0. 5ASD current density low current electrolysis for 8 hours, G. After laboratory analysis, the contents of sulfuric acid, copper sulfate and chloride ion in the tank were adjusted to the normal operation range, and the light agent was supplemented according to the results of Hall cell test. After the color of the electrolysis board is uniform, you can stop electrolysis, and then press 1-1. The current density of 5ASD was treated with electrolytic raw film for 1-2 hours, and a layer of black phosphorus film with uniform and dense adhesion was formed on the anode. I. Try plating OK. It can be done.

(5) the anode copper ball contains 0. 3Murray 0. The main purpose of 6% phosphorus is to reduce the anodic dissolution efficiency and reduce the production of copper powder.
.
7 the addition of chloride ion should be paid special attention, because the content of chloride ion is very low (30-90ppm), it must be accurately weighed in the measuring cylinder or measuring cup before it can be added; 1ml hydrochloric acid contains about 385ppm

Send Inquiry