Plastic electroplating - a brief description of the formula of plastic electroplating solution

Plastic electroplating - a brief description of the formula of plastic electroplating solution



Composition of solvent treatment solution: including cleaning: cleaning without dilute acid or neutral cleaning and 1-2% surface activator. Mix and immerse at 40-65 ℃ for 1-2 minutes.

Solvent treatment: with acetone, diacetate methane, and other active agents.

Conditioning: chemical roughening, chemical etching. Example 1 Anhydrous chromic acid cro3 20 g/l sulfuric acid h2so4 Specific gravity 1.84 600cc/l liquid temperature 60 ℃ time 15 to 30 minutes Example 2 Anhydrous chromic acid cro3 20 g/l phosphoric acid h3po3 100 cc/l sulfuric acid h2so4 500 cc/l Liquid temperature 69 ℃ time 10 to 20 minutes

Sensitizing: stannous chloride sncl2 20~40 g/l hydrochloric acid hcl 10~20 cc/l

Nucleation or activation Example 1 Palladium chloride pdcl2 0.1~0.3g/l Hydrochloric acid hcl 3~5 cc/l Example 2 Silver nitrate agno3 0.5~5 g/l Ammonia appropriate amount Example 3 Gold chloride aucl3 0.5~ 1 g/l hydrochloric acid HCl 1~4 cc/l