Improve plastic residual stress and improve electroplating performance (part 1)
The residual internal stress caused by injection molding is a killer that affects the electroplating performance of materials. In the previous article, the author conducted an in-depth analysis of how the internal stress affects the electroplating performance of the material. However, now that we understand the principle of its effect, we must know how to improve it. Starting from this issue, the author will conduct some further analysis on the improvement direction of residual stress in injection molding.
The topic of this issue-the direction of temperature improvement
The improvement of temperature on the residual stress of material injection is mainly divided into two aspects: injection molding temperature and mold temperature:
Injection molding temperature: Under the condition that the material will not crack, higher injection molding temperature can get better electroplating performance.
At a lower injection temperature, the fluidity of the material is poor, and the resistance during the filling process will increase. The molecular chains squeeze and stretch each other, resulting in serious molecular chain orientation after the part is cooled, so the injection molded The product will have greater internal stress; there is also the problem of deformation of the rubber phase in the material, which will eventually lead to uneven roughening and etching on the surface of the product, which will lead to poor appearance of the electroplated product and poor electroplating bonding force. .
At a higher injection temperature, the fluidity of the material is improved, the filling is smooth, and the stretch orientation between the molecular chains is slight. When the part is cooled, the molecular chain is basically in a natural curl state, so the injection residual internal stress of the part is also higher. Small, the electroplating performance of the material is greatly improved.
Related experiments show that for electroplated ABS materials, compared to products with injection temperature of 200-220℃, when the temperature is increased to 240℃-250℃, the adhesion of the coating increases by about 30% (see Figure 3 for details). At the same time, the defect rate of the surface appearance of the molded parts is also greatly reduced.

However, the injection temperature cannot be too high. If the material pyrolysis temperature is exceeded, the gas problem generated by the material pyrolysis will cause the appearance of the injection product surface to be poor, which will affect its electroplating performance.
Mold temperature: consistent with the direction of the material temperature, high mold temperature is conducive to improving the electroplating performance of the material.
In the state of low mold temperature, it is difficult to fill the material, the molecular chain orientation of the material is serious when the part is cooled, the internal stress of the product is large, and the electroplating performance is poor; on the contrary, under the state of high mold temperature, the material is filled smoothly, and the part is cooling When the molecular chain is basically in a natural curl state, the internal stress of the product is small, and the electroplating performance is greatly improved. The figure below is a schematic diagram of mold flow analysis of a part at different mold temperatures. It can be seen that when the mold temperature is 60 ℃, the maximum value of residual stress in different parts of the part reaches more than 40 MPa. When the mold temperature is 100 degrees Celsius, the maximum stress value of the part is relatively reduced, about 25MPa.

Ways to control mold temperature include ordinary water temperature controller, oil temperature controller, steam mold, E-mold, etc. The water temperature machine can generally realize the mold temperature control below 80℃, and the highest temperature does not exceed 90℃; the oil temperature machine can realize the mold temperature control of room temperature -300℃, but the commonly used range is 80-150℃; compared to the oil temperature machine , Steam mold and E-mold technology can not only achieve high mold temperature control, but also rapid cooling control. Therefore, when conditions permit, the use of oil temperature machine/steam mold/E-mold technology can greatly reduce the material's participation in internal stress, thereby improving the electroplating performance of the material.
At the same time, the actual mold temperature setting needs to be set in combination with the mold waterway and the requirements of the molding cycle. The mold temperature should be increased as much as possible without affecting other properties; while the mold temperature is controlled, the mold temperature must be maintained evenly. , Uneven mold temperature distribution will cause uneven shrinkage internal stress and affect electroplating performance. Uneven mold distribution and poor product structure design have the same effect on electroplating.
Conclusion: High injection molding temperature and mold temperature are beneficial to reduce the residual internal stress of the material and also improve the electroplating performance of the material. Correspondingly, the cooling time of the product in the mold will also increase, which will affect the production efficiency of injection molding. Therefore, for injection molding plants, the balance between stress residue and production efficiency is also one of their production troubles. In short, for electroplating materials, the editor still recommends that everyone try to use higher injection molding temperature and mold temperature.