Mar 09, 2024

Application of plastic plating-horizontal plating process in PCB plating

Application of plastic plating-horizontal plating process in PCB plating.
Huizhou Boluo Tenglong Technology Co., Ltd. serves you wholeheartedly! Mainly engaged in plastic hydroelectroplating processing, with plastic injection molding processing, mold processing and so on!
A brief introduction to the principle of horizontal plating.
The electrode reaction occurs after electrification, which makes the main components of the electrolyte ionized. the methods and principles of horizontal plating and vertical plating are the same, both must have negative and positive poles. The charged positive ions move to the negative phase of the electrode reaction zone, and the charged negative ions move to the positive phase of the electrode reaction zone, resulting in metal accumulation coating and gas release. Because the process of metal deposition in the cathode is divided into three steps: the hydration ion of the metal diffuses to the cathode; the second step is that the metal hydrate ion is gradually dehydrated when passing through the electric double layer and adsorbed on the surface of the cathode; the third step is that the metal ions adsorbed on the surface of the cathode accept electrons and enter the metal lattice. In the process of horizontal electroplating, the copper ions in the bath are transported to the cathode in three ways to form a double layer.
When electroplating, according to the theory of electrodeposition. The PCB located on the cathode is a non-ideal polarized electrode. The copper ions adsorbed on the surface of the cathode gain electrons and are reduced to copper atoms, which reduces the concentration of copper ions near the cathode. Therefore, a copper ion concentration gradient will be formed near the cathode. The bath in which the concentration of copper ion is lower than that of the main bath is the diffusion layer of the bath. On the other hand, the concentration of copper ion in the main plating bath is higher, which will be diffused to the place near the cathode where the concentration of copper ion is low, and replenish the cathode area from time to time. PCB is similar to a planar cathode, and the relationship between the current and the thickness of the diffusion layer is COTTRELL equation.
The limiting diffusion current depends on the concentration of copper ion in the main plating bath, the diffusion coefficient of copper ion and the thickness of the diffusion layer. When the concentration of copper ion in the main plating bath is high, the diffusion coefficient of copper ion is large, and the thickness of the diffusion layer is thin, it can be seen from the above formula. The greater the limiting diffusion current.
In order to achieve a higher limit current, it is known according to the above formula. Appropriate technological measures must be taken, that is, the technological method of heating must be adopted. Because increasing the temperature can increase the diffusion coefficient, increasing the convection rate can make it an eddy current and obtain a thin and uniform diffusion layer. From the above theoretical analysis, increasing the concentration of copper ion in the main plating bath, increasing the temperature of the plating bath and increasing the convection rate can increase the limit diffusion current. in order to accelerate the electroplating rate, the eddy current is formed by accelerating the convection speed of the plating bath, which can effectively reduce the thickness of the diffusion layer to about 10 microns. It is how to ensure the uniformity of the thickness of the copper layer on both sides of the substrate and the inner wall of the through hole. In order to obtain the uniformity of coating thickness, PCB plating is the key. It is necessary to ensure that the flow rate of the bath on both sides of the PCB and in the through hole is fast and consistent in order to obtain a thin and uniform diffusion layer.
In order to achieve a thin and uniform diffusion layer, according to the structure of the current horizontal plating system, although many nozzles are installed in the system, the plating solution can be quickly and vertically sprayed to the printed board to accelerate the flow speed of the plating solution in the through hole. as a result, the flow rate of the plating solution is very fast, and eddies are formed on and below the substrate and in the through hole, so that the diffusion layer is reduced and more uniform. But usually when the plating solution suddenly flows into the narrow through hole, the phenomenon of reverse reflux occurs at the entrance of the through hole, coupled with the influence of current distribution, which often leads to electroplating at the entrance hole, due to the tip effect, the thickness of the copper layer is too thick, and the inner wall of the through hole forms a copper coating in the shape of a dog bone. According to the state of the flow of the plating solution in the through hole, that is, the magnitude of eddy current and reflux, and the state analysis of the quality of the conductive plating through hole, the control parameters can only be determined by the process test method to achieve the uniformity of PCB plating thickness. Because the magnitude of eddy current and reflux is still not known by theoretical calculation, only the measured process method is adopted. It is known from the measured results that in order to control the uniformity of copper plating layer thickness of through hole, it is necessary to adjust the controllable process parameters according to the aspect ratio of PCB through hole, and even select copper plating solution with high dispersion capacity, and then add appropriate additives and improve the power supply mode, that is, reverse pulse current plating is used to obtain copper coating with high distribution ability.
Not only the horizontal plating system should be used for electroplating, but also the number of micro-blind holes in the laminate should be increased. Ultrasonic vibration should also be used to promote the replacement and circulation of the plating solution in the micro-blind hole, and then improve the power supply mode to adjust the controllable parameters by using the reverse pulse current and the actual test data, satisfactory results can be obtained.

Send Inquiry