Various undesirable phenomena of nylon injection molding:
Shrinkage, not fullness, unstable injection pressure
Generally, this situation is related to the small nozzle hole of the injection molding machine, because the nozzle is in long-term contact with the mold, the mold temperature is very low 20-90 ℃, and the nozzle temperature is 240-280 ℃. The temperature difference between them will inevitably lead to heat exchange. When the temperature of the nozzle drops below the melting point of nylon, the nozzle hole is frozen, and the next injection will have a large pressure to blow away, causing pressure loss and undershooting, but After increasing the injection pressure from time to time, the mold will expand after a few molds are produced.
From the perspective of the phenomenon, the injection molding machine is unstable. In fact, the nozzle hole is too small, and the phenomenon of increasing the nozzle hole will disappear.
Wavy flow mark
The generation mechanism is that the flow rate of the rubber material in the cavity is too slow, and the frozen rubber material has no way to stick to the mold.
Solution:
1. Increase the injection speed;
2. Increase the mold temperature;
3. Increase the temperature of the barrel;
4. Appropriately increase the nozzle aperture or gate.
Silver wire
The generation mechanism is that there is gas in the plasticized material, and the gas is forced out on the surface of the mold during injection, and white silk patterns appear on the surface of the product.
Solution:
1. Check if the raw materials are wet or mixed with other raw materials;
2. Check whether the raw materials are decomposed in the barrel (the temperature of the barrel is too high, and the screw speed is too fast);
3. Check whether the nozzle hole is too small;
4. Check whether the mold temperature is too low;
5. Poor mold exhaust;
6. Whether the gate size is too small;
7. The back pressure is too low and the recycled materials are used too much.
The generation mechanism is that the temperature of the rubber material at the end of the flow is very low, and the combination is poor and the pressure transmission is weak so that the two streams are not tightly combined.
Solution:
1. Increase injection pressure and speed;
2. Increase mold temperature;
3. Increase the material temperature;
4. Improve mold exhaust.