Reasons and solutions for the brittleness of the nickel plating brightener coating of plastic electroplating:
1. Solution for excessive main light agent: adjust the PH value of 3.0-3.5 electrolysis consumption
2. Solution to organic impurity pollution: treat with hydrogen peroxide and activated carbon
3. Solution to excessive metal impurities: add impurity remover
4. Solution to hexavalent chromium pollution: use insurance powder to deal with