What Is The Reason For The Uneven Thickness Of The Coating

Plastic plating-what is the reason for the uneven thickness of the coating? How to deal with it?
Huizhou Boluo Tenglong Technology Co., Ltd. serves you wholeheartedly! Mainly engaged in plastic hydroelectroplating processing, with plastic injection molding processing, mold processing and so on! .
Reason:

1 the anode distribution is incorrect.

(2) the design of the hanger is poor.
t01a30dad195470015e
Treatment method:

1 uniformly arrange the anode when mounting the parts.

(2) screen the parts correctly.
t01e888edd366f33e3c
Reason:

1 the dispersion ability of the plating bath is poor.

2 the bath temperature is high.

3The distance between electrodes is small.

(4) the product is suspended incorrectly in the slot.
t01e379f20269fe9d23
Treatment method:

1 add dextrin and sodium sulfate.

2 reduce the bath temperature.

3 increase the distance between electrodes.

(4) eliminate the incorrect suspension of the product.

 