Plastic Plating-Matrix Factors Affecting Adhesion
Huizhou City Boluo Tenglong Technology Co., Ltd. wholeheartedly serves you! Mainly engaged in plastic water electroplating processing, accompanying plastic injection molding processing, mold processing and so on!
It is self-evident that different coarsening processes, or different coarsening degrees of the same coarsening process, have an impact on the binding force. However, there are still some factors that will also affect the binding force of 83 plastic plating, and they are often easily ignored factors. These factors must be determined before the 633 plastic products that need to be plated are formed, otherwise the pass rate of plastic plating will be greatly reduced, and it will be difficult to find out the reasons. This is the composition ratio of the matrix material and the process conditions during injection molding.
As mentioned earlier, Liu plastic has a structure suitable for electroplating, but not all Ba-83 plastics are suitable for electroplating. Only electroplating grade, that is, Ba-83 plastics containing 8 components and about 20 ", are suitable for electroplating processing. Otherwise, the binding force is difficult to guarantee.
Some manufacturers entrust 833 products containing only 10X8 ingredients to electroplating factories for processing and electroplating. Not only is the product's binding strength unqualified, but it is also difficult to obtain a complete coating during the processing process. They can only rely on excessive coarsening and sacrificing surface finish. Plating out barely acceptable
Therefore, before electroplating eight plastics, it is necessary to confirm that the plastic used is plating grade. In case it is not plating grade, adjustments must be made in the roughening process to make the plating process go smoothly.
Even if plating grade VI-83 is used, it is sometimes found that it is not easy to plate, and quality problems such as poor bonding force may occur. The process parameters of all processes are within the effective range. At this time, we must look for plastic injection molding process problems.
During the injection molding process, plastic is in a hot flowing state and is subject to extrusion force, which will bring some changes to the composition of the plastic. Nowadays, some people have used microscopic process observation sensors to connect with computers to intuitively observe the flow characteristics of plastic (or metal) during the injection molding process, so as to better determine the injection molding process parameters.
The forming process factors that have been determined that affect the plateability properties of 838 plastics are as follows.
① The temperature test of plastic molding shows that high plastic molding temperature is conducive to the flow of plastic and can keep the distribution of plastic components in line with the design ratio. At the same time, it can reduce the deformation of the molded particles, maintain the roundness of the three components and increase the density of the plastic.
② Injection molding feeding speed should be as slow as possible, also to increase the roundness of the three components and increase the density of the plastic.
③ The pressure of injection molding feed should also be lower. This can prevent excessive internal stress caused by excessive pressure.
④ The temperature of the mold surface should be higher. This is conducive to the flow of the plastic material in the mold cavity and improves the density.
The injection molding process parameters of mature electroplated grade 883 plastic products are: the temperature of the molded plastic is 250.d egree. C. 0. The injection molding speed is 1.53, the injection molding pressure is 40 - 804 ‰ 1112, the mold temperature is 50 - 801, and the bonding force obtained by electroplating after appropriate roughening is 2.2 - 2^ 5^^. Claw.
After mastering the correct process parameters for injection molding, there are still some precautions to be taken seriously before injection molding, otherwise the adhesion of the coating will also be affected.
First, people 83 plastic should be de-moisture-treated. If the plastic is not dehumidified, defects such as air filaments, delamination, and small bubbles will remain on the surface of the plastic during injection molding. The moisture content of 633 is below 2, and the effect can be achieved by drying it with 8012. During drying, the accumulation of plastic in the oven shall not exceed 20~ 301X1X11.
Second, ensure the purity of raw materials and do not mix them with masterbatches, miscellaneous materials, dust, etc. At the same time, recycled plastic should not be mixed, otherwise it will affect the quality of plating.
Third, try to use little or no mold release agents. Because too much release agent facilitates product release, it makes it difficult to roughen electroplating. Especially for silicon release agents, it is best not to use them.
Fourth, the mold must be kept clean and there must be no residual plastic in the mold cavity. At the same time, to keep the mold cavity clean and tidy, it is best to polish or grind the mold cavity and then coat it with a metal that is easy to release, such as chromium, etc., on the premise of ensuring the product size requirements. This not only improves mold life, but also improves surface quality and makes it easier to release.