Huizhou Boluo Tenglong Technology Co., Ltd. serves you wholeheartedly! Mainly engaged in plastic hydroelectroplating processing, with plastic injection molding processing, mold processing and so on! .
In order to ensure the thickness of the coating, we should pay attention to the following five points in the construction:

The main results are as follows: (1) the anodizing time of materials with different purity should be controlled respectively. The film-forming rate of aluminum and its alloys with different purity is different, so the anodizing time should be treated separately. Usually, the lower the purity of aluminum is, the slower the film-forming speed is. Therefore, it is necessary to adjust the anodizing time reasonably according to the type of alloy.

(2) correctly calculate the area of anodized parts. The area of anodized parts must be calculated carefully, and the area of the fixture used should also be taken into account in the calculation, otherwise the input current density may be too large or too small. It is difficult to guarantee the thickness of the film.

(3) record the anodizing time correctly.

When the product hangs the anodizing tank, it is necessary to distribute the current immediately, and record the current delivery time and the product outlet time in time. When the constant current density anodization is used, the growth of the oxide film thickness is proportional to the time in a certain time, and the oxide film thickens gradually with the extension of time. If the time of entering and leaving the trough was not recorded at that time, the thickness of the film could not be guaranteed.

(4) the fixture contact should be firm and reliable. The poor contact between the parts and the fixture mainly occurs in the following two aspects.

1 between the parts and fixtures. When the elasticity of the fixture is poor, the cross-sectional area of the fixture is small, or there is an oxide film on the surface of the fixture, the contact resistance is increased, resulting in the fixture heating, which not only increases the power consumption, but also affects the smooth flow of the current. Before using the fixture, it is necessary to estimate the carrying capacity of the required current and fully clean it.

2 between the fixture and the anode copper stem. The poor contact between the fixture and the anode copper stem has its own unilateral reasons, and there are also two reasons. In short, the electrical conductivity test should be carried out after the fixture is in contact with the copper stem, and if no current is seen, it should be checked until the current is smooth.

(5) to prevent misunderstandings of calculation objects. The increase of the film thickness is related to the current density, and the film forming speed can be improved when the higher current density is used, which is independent of the voltage.