Plastic plating-full contact of multi-color electroplating process for plastic parts.
Huizhou Boluo Tenglong Technology Co., Ltd. serves you wholeheartedly! Mainly engaged in plastic hydroelectroplating processing, with plastic injection molding processing, mold processing and so on!
In recent years, daily necessities are constantly pushing through the old and bringing forth the new, which puts forward higher requirements for surface decoration. Multi-color electroplated ornaments are very popular among consumers and are widely used, ranging from signs, handicrafts to hardware, locks, lamps, glasses, clocks and so on. Plastic is a difficult plating material, although there are mature processes and many reports, but there are no reports on two-color electroplating and multi-color electroplating. At present, the processing price of some kind of plastic trademark electroplating (imitation gold + chromium) is as high as 89.9 yuan / dm2, which has a wide market and good benefit. This paper gives a brief introduction to the mature two-color electroplating process.
Technological process and matters needing attention.
De-stress "chemical deoiling" chemical coarsening "hydrochloric acid washing" colloidal palladium directly activated "ungluing" electroless nickel plating "brush washing" flash plating (pyrophosphate copper plating) "acid bright copper plating" bright nickel plating "dilute acid activation" gold plating passivation "drying" local point varnish "drying" removal of local imitation gold layer "dilute H2SO4 activation" chromium plating "drying" test. The washing process is omitted from the above process. But washing must be available, and it must be washed thoroughly. The washing after activation and degumming is strictly forbidden to rush with water. When operating each process, it is necessary to prevent abrasion and collision between the parts. The parts should be operated gently when the parts are loaded or poured out from the net or basket. it is best to pour them in a basin filled with water and use the buoyancy of water to prevent abrasions between the parts.
1 in addition to stress, put the plastic parts in the oven and keep them at 70 ℃ for 2 hours.
2 chemical deoiling.
40g/L Sodium hydroxide, Sodium Phosphate 30g/L, Sodium Carbonate 20g / L Diop emulsifier 1~3g/L, θ 60-70 ℃, t10~15min.
In the process of deoiling, the plastic parts should be stirred gently to speed up the deoiling speed. The coarsening recovery liquid can also be heated to no more than 70 ℃ to remove oil.
(3) Chemical coarsening [1] CrO3400g/L,H2SO4 (dice 1.84) 200ml pinch L; H2O600mL; relative density 1.45θ 70 ℃. As long as t10~15min is operated strictly according to this formula and working conditions, there will be no undercoarsening or excessive coarsening.
4Hydrochloric acid washing HCl (dumb1.19) 100ml / 200mL can remove residual coarsening liquid and adsorbed Cr3+ on plastic surface after hydrochloric acid washing for 3min. After washing with hydrochloric acid, the surface of the plastic can be observed with the naked eye from a light dark green to whiter.
(5) Colloidal palladium direct activation method PdCl2 ·2H2O0.5 ~ 1g/L, SnCl2 ·2H2O50 ~ 100g Mather HCl (dice 1.19) 200~300mL/L, θ 50 ℃ 60 ℃, t5~10min palladium chloride concentration should not be too high, otherwise the cost of trough configuration will be high and the loss will be high. In the formula reported in some materials [2], the mass concentration of palladium chloride is lower than that of 0.5g/L, which is proved to be not feasible in production. Even if the activation time is prolonged to above 30min and the temperature is raised to above 60 ℃, the exposed plastic will still appear, the production efficiency is low and the rate of finished product is low. In order to prevent the precipitation caused by the dilution of the activation solution caused by the introduction of cleaning water, before entering the colloidal palladium direct activation solution, the plastic parts were pre-soaked in the recovery solution after the colloidal palladium solution, and the colloidal palladium was activated directly without cleaning. It is forbidden to add and activate the unqualified nickel layer of plastic parts by electroless nickel plating directly into the colloidal palladium solution so as not to introduce the colloidal palladium activation solution into Ni2+, to reduce the activity and stability of the activation solution.
6. NaOH100~300g/Lt3~5min alkali solution is faster than acid solution in degumming speed, thoroughly and without heating, while acid solution needs more acid and heating.
(7) the composition, preparation, use and maintenance of electroless nickel plating, pyrophosphate copper plating, acid bright copper plating, bright nickel plating, imitation gold plating and chromium plating solution are the same as those of conventional plating bath.
There may be solid particles or other dirt on the surface of electroless nickel plating layer with brush brushing, which is easy to produce roughness and tattooing after electroplating, which is obvious on large area plating parts, so a brush brushing process is added. Do not use a hard brush when brushing, so as not to scratch the electroless nickel coating.
After gold plating with 9-point varnish, passivation and clear varnish can not only improve the anti-discoloration ability of the gold layer, but also play the role of insulation and prevent the gold layer from being plated with chromium again. Plastic parts are not heat-resistant, so transparent varnish is required to be self-drying at room temperature or low temperature drying. Local point transparent varnish should be careful, to prevent the need for chromium-plated patterns on the paint. If you need to dry the paint film, the temperature should not exceed 70 ℃.
Concluding remarks.
The market prospect of multicolor electroplating is promising and the benefit is good, but there is no report for reference when it starts late. The two-color electroplating product introduced in this paper, the golden yellow (imitation gold) background sets off the white bright (chromium) pattern pattern, the appearance is very beautiful. However, the bright nickel layer takes more than 24 hours after many processes, such as gold plating, passivation, drying, spot varnish, drying, partial removal of the gold coating and so on. Although the dilute H2SO4 is soaked and activated for a long time, the qualified rate of chromium plating is still too low (about 40%), which restricts the economic benefits. It is believed that with the efforts of electroplating workers, others such as satin nickel + imitation gold, black nickel + imitation gold, red bronze + black nickel, white nickel + black nickel + gold, red bronze + black nickel + imitation gold. The multi-color electroplating process will be more mature.