In the process of plastic electroplating, many steps are used, and a little careless operation or inspection may lead to defects in the final product. Understanding some common causes of defects can help reduce defects and improve product yield.
Now let’s go through the factors that lead to defective plating products.
gap
Reason: There are cracks or marks on the plastic surface, resulting in the residual moisture in the plastic entering the surface during the electroplating process, forming a crack.
flash
Reason: Excess plastic or uncleanly falling out of the mold causes the plastic edge to protrude, which becomes sharp during the molding process, which affects the appearance and is not noticed until after plating.
blister
Reason: It may be caused by the bubbles generated between the metal deposition layer during the electroplating process, or it may be caused by the plastic and the metal deposition layer caused by the moisture contained in the plastic. Need to cut open the blisters for testing before identification.
Scratches and dents
Reason: Scratches and dents produced during molding or processing (raw materials or electroplated parts) did not appear immediately, entering the electroplating process, or scratching the original parts during the processing. The depth of the scratches or dents and the plating deposits on the area can be used to determine whether the defect is superficial or in the substrate.
Dry up
Cause: It is caused when the part becomes too dry between the metal deposits during the electroplating process. This situation can be avoided by careful process control of the electroplating operation.
Warpage
Reason: The size of the component is deformed during the production process, which may be caused by molding errors, or it may be due to exposure to extreme temperatures, or it may be caused by incorrect handling of components.
springboard
Reason: The substrate is not completely immersed in the plating solution, or there are contaminants on the surface of the substrate. Ensure that the substrate is completely immersed and cleaned, which can reduce the occurrence of springboards.